Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: https://dspace.ncfu.ru/handle/123456789/27101
Название: SYNTHESIS AND CHARACTERIZATION OF SELENIUM NANOPARTICLES STABILIZED WITH DIDECYLDIMETHYLAMMONIUM CHLORIDE
Другие названия: СИНТЕЗ И ХАРАКТЕРИСТИКА НАНОЧАСТИЦ СЕЛЕНА, СТАБИЛИЗИРОВАННЫХ ДИДЕЦИЛДИМЕТИЛАММОНИЯ ХЛОРИДОМ
Авторы: Blinov, A. V.
Блинов, А. В.
Blinova, A. A.
Блинова, А. А.
Rekhman, Z. A.
Рехман, З. А.
Gvozdenko, A. A.
Гвозденко, А. А.
Golik, A. B.
Голик, А. Б.
Kolodkin, M. A.
Колодкин, М. А.
Oblogin, Y. A.
Облогин, Я. А.
Ключевые слова: Aggregative stability;Surfactants;Dynamic light scattering;Selenium nanoparticles;pH
Дата публикации: 2024
Библиографическое описание: Blinov, A.V., Blinova, A.A., Rekhman, Z.A., Gvozdenko, A.A., Golik, A.B., Kolodkin, M.A., Oblogin, Ya.A. SYNTHESIS AND CHARACTERIZATION OF SELENIUM NANOPARTICLES STABILIZED WITH DIDECYLDIMETHYLAMMONIUM CHLORIDE // ChemChemTech. - 2024. - 67 (4), pp. 46-52. - DOI: 10.6060/ivkkt.20246704.6938
Источник: ChemChemTech
Краткий осмотр (реферат): As part of this work, a synthesis procedure was developed and the characteristic of selenium nanoparticles stabilized with didecyldimethylammonium chloride (DDAC) was carried out. Nano-particles were obtained by chemical reduction in an aqueous medium. Selenous acid was used as a selenium-containing precursor, ascorbic acid was used as a reducing agent, and didecyldime-thylammonium chloride was used as a stabilizer. To determine the optimal parameters for the synthesis of selenium nanoparticles stabilized with didecyldimethylammonium chloride, a multifactorial experiment was carried out. The input parameters were the concentration of selenous acid, the concentration of didecyldimethylammonium chloride (DDAC) and the concentration of ascorbic acid. The average hydrodynamic radius of selenium particles, which was determined by the method of dynamic light scattering, was considered as an output parameter. The optimal parameters for the synthesis of selenium nanoparticles (R from 15 to 25 nm) have been established: reducing agent concentration – from 1.076 mol/l to 2.118 mol/l, stabilizer concentration – from 0.006 mol/l to 0.085 mol/l, precursor concentration – from 0.004 mol /l to 0.236 mol/l. At the next stage of research, the effect of solution pH on the average hydrodynamic radius of selenium nanoparticles was determined. It was shown that in the pH range from 1.81 to 2.21, the average hydrodynamic radius of selenium nanoparticles does not change significantly, which indicates the aggregative stability of selenium nanoparticles in this range. In the pH range from 2.21 to 4.56, there is a sharp increase in the average hydrodynamic radius from 21 to 497 nm. At pH ˃ 7.96, coagulation of selenium particles is observed.
URI (Унифицированный идентификатор ресурса): https://dspace.ncfu.ru/handle/123456789/27101
Располагается в коллекциях:Статьи, проиндексированные в SCOPUS, WOS

Файлы этого ресурса:
Файл Описание РазмерФормат 
scopusresults 3050 .pdf
  Доступ ограничен
134.66 kBAdobe PDFПросмотреть/Открыть
WoS 1859 .pdf
  Доступ ограничен
123.59 kBAdobe PDFПросмотреть/Открыть


Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.