Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: https://dspace.ncfu.ru/handle/123456789/34213
Название: Influence of Sintering Additive Type on the Optical Properties of YAG:Ru Ceramics
Авторы: Suprunchuk, V. E.
Супрунчук, В. Е.
Chapura, O. M.
Чапура, О. М.
Kravtsov, A. A.
Кравцов, А. А.
Malyavin, F. F.
Малявин, Ф. Ф.
Lapin, V. A.
Лапин, В. А.
Tarala, L. V.
Тарала, Л. В.
Bedrakov, D. P.
Бедраков, Д. П.
Vakalov, D. S.
Вакалов, Д. С.
Ключевые слова: Additives;YAG:ru;Color centers;Photochromism;Photoluminescence;Ruthenium compounds;Ceramic;MgO;SiO 2;Valence conversion;Sintering additives;Optical properties
Дата публикации: 2026
Издатель: John Wiley and Sons Inc
Библиографическое описание: Suprunchuk V. E., Chapura O. M., Kravtsov A. A., Malyavin F. F., Lapin V. A., Tarala L. V., Bedrakov D. P., Vakalov D. S. Influence of Sintering Additive Type on the Optical Properties of YAG:Ru Ceramics // Journal of the American Ceramic Society. - 2026. - 109 (8). - art. no. e71121. - DOI: 10.1111/jace.71121
Источник: Journal of the American Ceramic Society
Краткий осмотр (реферат): Ruthenium-doped yttrium aluminum garnet (YAG:Ru) ceramics were synthesized by chemical precipitation. The effects of sintering conditions and the amount and type of sintering additives on the optical properties of YAG:Ru ceramics were investigated. A comparative analysis of the optical properties and color centers was performed as a function of the concentrations of Mg2+, Ca2+, and Si4+ cations. It was found that the maximum linear light transmittance (72% at 1100 nm) was achieved with the addition of MgO or CaO at sintering temperatures of 1800°C and 1825°C, respectively, whereas the use of SiO2 resulted in a lower transmittance of 58% at 1850°C. The color of the samples varied from red (without additives, with SiO2, and with high concentrations of CaO) to gray (with MgO and CaO 0.05 wt%), which could be associated with the formation of different color centers. Several absorption bands in the visible and near-IR range were found for the YAG:Ru ceramic samples: approximately 2130 nm (0.58 eV, for the sample containing CaO), approximately 1348 nm (0.92 eV, without additives and with SiO2), approximately 585 nm (2.11 eV, without additives), and bands at approximately 450–465 nm and approximately 340 nm (2.75–2.67 and 3.65 eV, respectively, for all samples). Two narrow bands at 648 and 672 nm were detected in the photoluminescence spectra under excitation at 310 nm. These bands appeared in samples with CaO, MgO, and even in undoped YAG, but disappeared upon the introduction of SiO2. These results open the possibility of controlling the optical properties of YAG:Ru ceramics by varying the type of sintering additive, revealing potential applications in laser and photochromic systems.
URI (Унифицированный идентификатор ресурса): https://dspace.ncfu.ru/handle/123456789/34213
Располагается в коллекциях:Статьи, проиндексированные в SCOPUS, WOS

Файлы этого ресурса:
Файл Описание РазмерФормат 
scopusresults 4095.pdf
  Доступ ограничен
121.96 kBAdobe PDFПросмотреть/Открыть
WoS 2387.pdf
  Доступ ограничен
111.69 kBAdobe PDFПросмотреть/Открыть


Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.